INCURE UV Light Curable Decorative & Dome Coatings are ideal for badges, decals, nameplates, keychains, pens. These one part, no-mix products cure in seconds for immediate inspection in high assembly operations.

        

        


 Cast-MaxTM

Product Description Color Tensile Viscosity Hardness Elongation
2613 Low viscosity bonder. Used in gems and metal bonding for bracelets, necklaces, rings, penchants, hair clips, hair bands, earrings, crowns etc. Also used as dome coating of nameplates and logos. Clear 4,700 - 5,200 psi 700 - 1,400 cps D83 - D93 30%
2664 Medium viscosity bonder. Used in gems and metal bonding for bracelets, necklaces, rings, penchants, hair clips, hair bands, earrings, crowns etc. Also used as dome coating of nameplates and logos. Clear 4,700 - 5,200 psi 2,000 - 4,000 cps D79 - D89 30%