GENERAL PURPOSE CYANOACRYLATE

Product  Description Color Viscosity Tensile Specific Gravity Chemical Type
101 Low viscosity cyanoacrylate adhesive. Fast setting wicking grade adhesive ideal for bonding preassembled parts. Clear 2 cps 3,400 psi 1.06 Ethyl
104 Low to medium viscosity cyanoacrylate adhesive. Suitable for general-purpose applications on metals, rubbers, or plastics.  Clear 100 cps 3,400 psi 1.06 Ethyl
105 Low to medium viscosity cyanoacrylate adhesive. Suitable for general-purpose applications on metals, rubbers, or plastics.  Clear 10,000 cps 3,875 psi 1.06 Ethyl
115 High viscosity cyanoacrylate adhesive that is ultra fast setting. Suitable for general-purpose applications on metals, rubbers, or plastics.  Clear 1,500 - 2,000 cps  3,400 psi 1.06 Ethyl
117 A medium viscosity cyanoacrylate adhesive that is fast setting and ideal for rubber and plastic bonding applications. Clear 150 - 250 cps 3,875 psi 1.06 Ethyl