HIGH TEMPERATURE EPOXY

Product Color Viscosity Ratio Tensile Flexural Strength Cure Shrinkage Dielectric Strength Temp. Resistance
HTE-5350 Grey Paste 1:1 2,500 psi 11400  psi 0.002 in/in 80 volts/mil -65 to 204 °C
HTE-5351 Amber 25,000 cps 1:1 3,000  psi 10,200  psi 0.002 in/in 440 volts/mil -65 to 204 °C
HTE-5352 Grey Paste 1:1 2,500  psi 12,000  psi 0.002 in/in N.D. -65 to 204 °C
HTE-5353 Grey 75,000 cps 1:1 1,135  psi - 0.009 in/in 380 volts/mil -55 to 130 °C
HTE-5354 Clear 12000 cps 1:1 1,200  psi 8,000  psi 0.008 in/in 860 volts/mil -50 to 200 °C
HTE-5355 Light Grey Paste 100:13 2,350  psi 11,800  psi 0.004 in/in 460 volts/mil -65 to 204 °C
HTE-5356 Black 3,000 cps 100:25 - 12,300  psi 0.003 in/in 480 volts/mil -55 to 185 °C
HTE-5357 Black 16,000 cps 100:12 1,135  psi 14,100 0.003 in/in 460 volts/mil -55 to 120 °C