ULTRA HIGH TEMPERATURE EPOXY

Product Description Color Dielectric Strength Viscosity Hardness Volume Resitivity
UHTE-5320 Two Part Epoxy, 1:1 Ratio System for Tough Bonding Applications. Amber 450 volts/mil 8,500 cps D89 4.0 x 1014
UHTE-5321 Single-Part Contact Adhesive, Excellent Flexibility. Black 300 volts/mil 35,000 cps N.D. 1.0 x 1013
UHTE-5322 Two Part Epoxy, 100:12 Ratio. Aluminum-Filled, Ultra High-Temp, Low Shrinkage and High Thermal Conductivity. Grey 50 volts/mil 11,000 cps D87 1.0 x 105