THERMALLY CONDUCTIVE GREASE

Product Filler Color Chemical Resistance Thermal Conductivity Specific Gravity Dielectric Strength Volume Resistivity
TCG-10 Alumina White Excellent 0.475 W/m-°K 2.42 gms/cc 300 volts/mil 1014
TCG-20 Aluminum Nitride Grey Excellent 2.23 W/m-°K 2.27 gms/cc 300  volts/mil 1014
TCG-30 Aluminum Aluminum Excellent 3.04 W/m-°K 1.35 gms/cc 40  volts/mil 104
TCG-40 Copper Copper Excellent 4.68 W/m-°K 1.33 gms/cc 4  volts/mil 103