UV CURE SILICONE

Product Color Viscosity Cure System Surface Dry Time Cure Time Tensile Temp. Resistance
901 Clear 7,000 cps UV Light + Moisture 5 sec. UV 24 hr, RT 100 psi -45 to 260 °C
904 Clear 2,500 cps UV Light + Moisture 5 sec. UV 24 hr, RT 80 psi -45 to 260 °C
905 Clear 600 cps UV Light + Moisture 5 sec. UV 24 hr, RT 100 psi -45 to 260 °C
909 Clear 3,000 cps UV Light + Moisture 5 sec. UV 72 hr, RT 100 psi -45 to 260 °C
915 Straw 100,000 cps UV Light + Moisture 5 sec. UV 72 hr, RT 500 psi -45 to 260 °C
917 Straw 45,000 cps UV Light + Moisture 5 sec. UV 72 hr, RT 200 psi -45 to 260 °C