THREADLOCKERS

Product Description Color Viscosity Gap Fill Strength Break Torque
10 Low strength. For threadlocking on collars, screws, pulleys etc. Recommended for metals such as aluminum and brass.  Purple 5,000 cps 0.007 Low 25 - 70
25 Medium strength. Lock and seal metal fasteners. For applications where disassembly with hand tools is required for servicing.  Blue 1,200 - 2,000 cps 0.007 Medium 70 - 150
27 Thixotropic. Medium strength. Surface-insensitive, works effectively without primer, as well as on oily or otherwise contaminated metal surfaces. Blue 3,000 cps 0.007 Medium 120 - 170
49 Low viscosity. High strength. Suitable for heavy-duty applications where high levels of shock, vibration and stress are present.   Red  400 - 600 cps 0.007 High 140 - 320
50 High viscosity. High strength. Suitable for large assemblies and heavy- duty applications where high levels of shock, vibration and stress are present.  Red  5,500 - 8,000 cps 0.016  High 150 - No Limit
70 Low viscosity. Develops medium to high strength. Seals porosities in welds and castings. Green 30 cps 0.003 High 150 - No Limit