UV LIGHT CURING CONFORMAL COATING

Ultra-IlluminaTM

Product Description Color Water Absorption Viscosity Hardness Elongation
3502 Low viscosity, hard and resilient UV curable conformal coating (30-150 microns) for PCBA. Use with high volume spray valve system, does not clog valves. Fluorescing feature for in-line inspection. Clear 0.01% 300 - 400 cps D35 - D45 74%
3511 Low viscosity, clear, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA. Shadowed areas under components are cured with secondary heat-cure process. Clear 0.9% 100 - 200 cps D55 - D75 7%
3511B Low viscosity, black, opaque, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA. Shadowed areas under components are cured with secondary heat-cure process. Black 0.9% 110 - 210 cps D75 - D85 7%
3561 Very low viscosity, hard and resilient UV curable conformal coating (30-150 microns) for PCBA. Use with high volume spray valve system, does not clog valves. Fluorescing feature for in-line inspection. Clear 0.01% 150 - 300 cps D35 - D45 74%