LIGHT-CURABLE FOR ELECTRONICS ASSEMBLY

Metal Bonder
Product Description Color Viscosity Tensile Hardness Elongation
1283 Cures with UV / Visible /  Heat or Actif 398. Good clarity, heat and moisture resistance. Good passive vibration isolation capability. Ideal for relays for circuit breakers in the electronics industry for outdoor use. Clear 400 - 800 cps 5,700 - 9,800 psi D68 - D78 55%
1203 Cures tack-free with up to 5,400 PSI on many different metals / glass /  ceramics. Very low linear shrinkage with enhanced excellent moisture and temperature resistance. Good passive vibration isolation capability. Clear 500 - 900 cps 4,400 - 5,400 psi D59 - D69 400%
Plastic Bonder
Product Description Color Viscosity Tensile Hardness Elongation
1462 Low viscosity, acid-free, multi-substrate / plastic bonder. For electronics industry. Good bonding strength on multiple substrates such as metals, glass and FR4 materials on a single application. Slightly Amber 300 - 600 cps 2,800 - 6,900 psi D49 - D59 827%
1483 Medium viscosity, acid-free, multi-substrate /  plastic bonder. For electronics industry. Good bonding strength on multiple substrates such as metals, glass and FR4 materials on a single application. Slightly Translucent   700 - 1,600 cps 2,800 - 7,000 psi D55 - D65  915%
1063 Medium viscosity, acid-free, multi-substrate / plastic bonder. For electronics industry. Good bonding strength on multiple substrates such as metals, glass and FR4 materials on a single application. Clear 1,800 - 3,200 cps 3,300 - 7,000 psi D58 - D68 380%
Potting
Product Description Color Viscosity Tensile Hardness Elongation
3339 Very thick, low water absorption electronics sealant. Provides air-tight seal with ease of peel for rework. Tough yet elongating. Widely use for automotive and electronics industries for its low CTE properties. Slight Translucent 27,000 - 50,000 cps 1,100 - 3,400 psi A12 - A22 71%
6228HT Cost efficient epoxy-acrylate, thick viscosity, ultra-low shrinkage and water absorption potting compound for use in sensitive electronic devices. UV / Heat curable. Chemical and vapor resistance. Clear 5,000 - 8,000 cps 1,700 - 5,600 psi D55 - D65 160%
6213 Cost efficient epoxy-acrylate low viscosity, ultra-low shrinkage and water absorption potting material for use in sensitive electronic devices. Chemical and vapor resistance.  Transparent 500 - 1,200 cps 2,200 - 2,700 psi D55 - D65   210%