UV GLASS BONDING ADHESIVES

Glass + Crystal
Product Description Color Viscosity Tensile Hardness Elongation
1931 Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics bonder. Low linear shrinkage, good weather-ability, temperature and moisture resistance. Slight Tint 80 -180 cps  7,400 - 10,000 psi D75 - D85 0.04%
5235 Medium viscosity medical bonder. Extra-ordinary high bonding strength to metals, glass and ceramics. Very low linear shrinkage and low water absorption with good thermal and moisture resistance. Clear 3,000 - 6,000 cps 6,100 - 8,300 psi D75 - D85 0.03%
1203 Cures tack-free with up to 5,400 PSI on many different metals / glass / ceramics. Very low linear shrinkage with enhanced excellent moisture and temperature resistance. Good passive vibration isolation capability.   Clear  400 - 800 cps  4,400 - 5,400 psi D59 - D69  4%
Glass + Metal
Product Description Color Viscosity Tensile Hardness Elongation
1238 Very high strength, high viscosity metal / glass bonder. Very low water absorption and linear shrinkage. Fast-curing and ideal for bonding all types of glass panels to stainless steel structures in general industries.  Clear 16,000 - 26,000 cps 5,700 - 8,900 psi D75 - D85 0.76%
9263 Cures with UV / Visible / Heat or Actif 398. Very high strength, low viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption. Slight Tint 500 - 1,000 cps 6,500 - 16,000 psi D67 - D77 5.1%
9245 Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption.   Slight Tint 2,500 - 4,800  cps  6,800 - 10,000 psi D65 - D75  8.2%
1922 Cures with UV / Visible / Heat or activator (Actif 398). Low viscosity and high strength metal / glass / ceramics bonder. Very low shrinkage and good weather-ability, temperature and moisture resistance. Slight Tint 250 - 500  cps  9,700 - 10,900 psi D77 - D87  0.04%
Glass + Metal + Plastic
Product Description Color Viscosity Tensile Hardness Elongation
1471 Industrial grade, very low viscosity high strength multi-substrate bonder. Very useful for bonding of substrates with different hardness.  Clear Translucent 80 - 170 cps 2,400 - 6,800 psi D68 - D78 3.1%
1859 Multi-substrate bonding gel for most plastics, metal and glass. Ideal for out-door bonding in general and construction industries. Good passive vibration resistance. Enhanced thermal and water resistance  Clear 38,000 - 68,000 cps 3,700 - 6,900 psi D63 - D73 2.6%
Thank You! Your message has been sent. Something went wrong, please try again later. Please enter a correct Captcha answer.