LIGHT CURABLE PEELABLE MASKS

LitemaskTM 

Product Description Color Viscosity Tensile Hardness Elongation
4201
Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance.
Slight Tint
80 - 180 cps 7,400 - 10,000 psi D75 - D85 4%
4272
Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance.
Slight Tint
250 - 550 cps 9,700 - 10,900 psi D77 - D87 4%
4153 Ultra-clear, low viscosity UV / Visible Light / LED / Activator / Heat-curing, high strength metal-glass mask for protection of surfaces during blasting. Remove by burn-off. Tack-free, used in jewelry industry. Slightly Translucent 500 -900 cps 7,000 - 8,400 psi D66 - D76 33%
3148 Ultra-clean and tough. Very effective protection against chemical stains and scratch marks. No residue or contamination after removal. Ideal for protection of critical surfaces during manufacturing processes. Dark Blue 4,000 - 8,000 cps 4,600 - 5,300 psi D49 - D59 250%
1128 Very high viscosity and clear peel-able mask for temporary protection of components. Protection against soldering and sand-blasting processes. Remove by soaking in hot water. Highly elongation and very tough material. Clear 18,000 - 32,000 cps 5,000 - 6,900 psi D67 - D77 300%
4139 Cures with UV / Visible / Heat or Actif 398. Very good adhesion to metals and glass. Used in aerospace industry for the effective protection of turbine blades against chemicals during cleaning. Clear Gel 9,800 - 16,000 psi D68 - D78 55%
8177G
Gel form, ultra-clean peel-able high temp mask for electronics and aerospace industries. Soft, tough and flexible for surface protection against chemical stains and burnt marks during manufacturing processes.
Clear Blue
Gel 3,600 psi A15 - A25 184%