OPTICAL ASSEMBLY ADHESIVES

OptikTM

Product Description Color Viscosity Tensile Hardness Elongation
7210 Very low viscosity sealant for optical devices. Ultra-low linear shrinkage. Ideal for optical positioning / alignment with excellent passive vibration resistance capability. Bonds very well to glass / metals / ceramics / plastics. Slight Yellowish Tint 10 - 150 cps 2,600 - 7,000 D24 - D34 477%
7760 Very low viscosity active alignment optical bonder. Used in optical / medical devices for bonding of metals, glass and ceramics. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling. Slight Tint 60 - 120 cps 8,700 - 10,100 D83 - D93 11%
7731 Very low viscosity active alignment optical bonder. Used in optical / medical devices for bonding of metals, glass and ceramics. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling. Slight Tint 150 - 350 cps 8,000 - 10,600 D83 - D93 7%
1722 High precision active alignment bonding of micro-devices. Multi-substrates high-precision optical bonder. Designed with enhanced excellent moisture and temperature resistance to pass standard thermal cycling tests. High Clarity 400 - 750 3,200 - 3,900 D25 - D35 1500%
7063 Cures tack-free with up to 5,400 PSI on many different metals / glass / ceramics. Very low linear shrinkage with enhanced excellent moisture and temperature resistance. Good passive vibration isolation capability. Clear 500 - 900 cps 4,400 - 5,400 D59 - D69 400%
7863 Optical grade, multi-substrate bonder for plastics  / metal / glass. Ideal for furniture / jewelry / home appliances in general and construction industries. Enhanced thermal and water resistance.  Clear Translucent  1,200 - 2,100 cps  4,000 - 5,700  D65 - D75 70%
7214 Medium viscosity bonder for optical devices. Chemical resistant and does not yellow over prolonged exposure to the environment. Ideal for optical positioning / alignment, it bonds well to various substrates. Slight Yellowish Tint 1,800 - 3,800 cps 1,180 - 3,630 D47 - D57 788%
7664 Medium viscosity active alignment optical bonder. Used in optical / medical devices for bonding of metals, glass and ceramics. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling. Slight Tint 2,000 - 4,000 cps 6,400 - 10,900 D83 - D93 18%
7795 Medium high viscosity, superior high strength bonder. Used for bonding of metals, glass and ceramics in electronics / optical / medical devices. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling. Slight Tint 5,000 - 8,000 cps 10,100 - 12,600 D82 - D92 24%
Thank You! Your message has been sent. Something went wrong, please try again later. Please enter a correct Captcha answer.