PLASTIC BONDING ADHESIVES

Uni-WeldTM

 

PVC
Product Description Color Viscosity Tensile Hardness Elongation
1013 Industrial grade, high strength plastic bonder for Ultem, PVC and many different plastics. Ultem, PVC and many different plastics. Slight Yellow Tint 800 - 1,500 cps 7,100 D68 420%
1095 Medium viscosity low cost bonder. Cures tack-free in seconds. Excellent choice for applications requiring good bonding strength on various types of plastics. Used in high volume production. Clear 4,000 - 7,000 cps 5,800 D73 - D83 35%
1453 Uniquely high elongation provides extra-ordinary bonding of different hardness layers for the construction of sport-courts, cushion carpets etc. High strength plastics bonder with good vibration isolation capability. Slight Yellow Tint  500 - 900 cps  6,900 D45 - D55  860%
1465 Cures tack-free, it is a superior plastics / metals /  glass / ceramics multi-substrate bonder. Ideal for applications requiring minimal drift in positioning optics and devices with very low shrinkage property.  Slight Translucent 4,000 - 8,000 cps 5,400  D60 - D70 105%
1832VT Industrial grade, multi-substrate, high viscosity and very low linear shrinkage bonder for many plastics / metal / glass. Ideal for applications requiring bonding of dissimilar substrates.  Clear Translucent  7,000 - 15,000 cps 7,100  D63 - D73  320%
PET / APET
Product Description Color Viscosity Tensile Hardness Elongation
1417 Industrial grade, high strength plastic bonder for Ultem, PVC and many different plastics. Use in the sealing of test-tubes. Formulated to meet ISO 10993-5. Passes EtO and gamma sterilization. Slight Yellow Tint 6,000 - 12,000 cps 6,000 A45 - A55 235%
1072 Low viscosity low cost bonder. Cures tack-free in seconds. Excellent choice for applications requiring good bonding strength on various types of plastics. Used in high volume production. Slight Tint 300 - 600 cps 7,000 D76 - D86 13%
1859 Multi-substrate bonding gel for most plastics, metal and glass. Ideal for out-door bonding in general and construction industries. Good passive vibration resistance. Enhanced thermal and water resistance Clear  38,000 - 68,000 cps  6,900 D63 - D73  110%
Nylon, LCP
Product Description Color Viscosity Tensile Hardness Elongation
1054 Ultra-fast curing industrial bonder for many different plastics such as PC / PVC / Elastomers. Extremely high bonding strength, low linear shrinkage and water absorption. Ideal for applications requiring thermal cycling. Slight Yellow Tint 1,500 - 3,500 cps 10,800 D70 - D80 60%
1403 Low viscosity high strength plastics bonder. Also bonds to metals / glass / ceramics. Low water absorption and linear shrinkage. Suitable for products requiring thermal cycling with good temperature resistance. Slightly Amber 500 - 1,200 cps 7,800 D65 - D75 150%
PC, ABS
Product Description Color Viscosity Tensile Hardness Elongation
1404 Medium viscosity, acid-free form-in-place gasket and sealant. Very low linear shrinkage. Ideal for medical optics positioning / alignment application. Adhere well to glass / metals / ceramics / plastics. Slight Yellow Tint 2,000 - 3,800 cps 7,100 D67 - D77 73%
1435 A very fast curing, high strength plastic bonder for PVC / PC / ABS / Polyester / Ultem and many different plastics. Highly flexible, it is used also in the sealing of test-tubes. High temperature and thermal resistance. Slight Yellow Tint 3,200 - 5,800 cps 7,300 D55 - D65 240%
1832 UV / Visible light curing, multi-substrate, low viscosity, low water absorption bonder for plastics / metal / glass. Ideal for applications requiring bonding of dissimilar substrates. Clear  200 - 400 cps  6,900 D60 - D70  350%