115-500GM
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Fast setting, High viscosity, Solvent-resistant and Bonds P,R,M,F,C,W
Substrates : High Strength, Multi-Substrates Structural CA Bonder
Viscosity : 1,800 cps
Shear Strength : 3,400 psi
Bonding Strength (psi)
ABS : 2,400
Aluminum : 2,300
PC : 3,400
PVC : 3,400
Rubber : 2,200
Steel : 3,000