THERMALLY CONDUCTIVE GREASE

HIGH PERFORMANCE THERMALLY CONDUCTIVE GREASE

Incure Thermal Greases are ceramic and metal-filled silicone systems which offers exceptional thermal and electrical properties to 550°F. These thermally conductive grease offers good thermal conductivity and are used in aluminum heat sinks, ballast resistors, heat pipes, high-power electronic devices and other heat exchange systems.

Advantages of Incure Thermally Conductive Epoxy

  Good Thermal Conductivity
  Ceramic and Metal-Filled Silicone Systems
  Exceptional Thermal and Electrical Properties to 550°F


Learn about our Light Curing Systems

C9000 / U8000 UV Light Curing Conveyor Systems
F100P / F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED Flood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps
Repair Heat Pipes

Core Products
Product Filler Color Chemical Resistance Thermal Specific Dielectric Volume Temperature  
Conductivity Gravity Strength Resistivity Limit  
W/m-°K gms/cc volts/mil Ohms-cm °F  
TCG-10 Alumina White Excellent 0.475 2.42 300 1014 -60 to 550
TCG-20 Aluminum Nitride Grey Excellent 2.23 2.27 300 1014 -60 to 550
TCG-30 Aluminum Aluminum Excellent 3.04 1.35 40 104 -60 to 550
TCG-40 Copper Copper Excellent 4.68 1.33 4 103 -60 to 550
Package Size: Pint / Quart / Gallon

Results 1 - 4 of 4
TCG-40

Filler                                          ...

TCG-30

Filler                                          ...

TCG-20

Filler                                          ...

TCG-10

Filler                                          ...