UV GLASS BONDING ADHESIVES FOR GLASS & INDUSTRIAL ASSEMBLY
Incure glass glue cure in seconds upon exposure to UV light. These cutting edge UV light-curing adhesives are particularly designed for decorative and industrial glass assembly. Suitable for glass to glass, glass to metal, glassware bonding, acrylic glass, crystals, tempered glass, etc.
Advantages of Quad-CureTM - UV Glass Adhesives
Cure In Seconds! Invisible Bond Excellent Adhesion Environmetally Resistant Superior Performance
Advantages of Quad-CureTM - UV Glass Adhesives
Cure In Seconds! Invisible Bond Excellent Adhesion Environmentally Resistant Superior Performance
Quad-cureTM Series Core Products (Glass, Crystals)
Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics bonder. Low linear shrinkage, good weather-ability, temperature and moisture resistance.
Very low Viscosity, UV / Visible light / LED / Heat-curing, high strength metal-glass bonder. Track free,used in very high strength bonding application requiring good temperature and moisture resistance.
Cures with UV / Visible / Heat or Actif 398. Very high strength, medium viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption
Cures with UV / Visible / Heat or Actif 398. Very high strength, low viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption.
Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption.
Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption.
Cures with UV / Visible / Heat or activator (Actif 398). Low viscosity and high strength metal / glass / ceramics bonder. Very low shrinkage and good weather-ability, temperature and moisture resistance.
High Performance Metal / Glass / Ceramics
Slight Tint
375 cP
9,700 to 10,900
D77 – D87
4%
Quad-cureTM Series Core Products (Glass + Metal + Plastic)
Very high strength, high viscosity metal / glass bonder. Very low water absorption and linear shrinkage. Fast-curing and ideal for bonding all types of glass panels to stainless steel structures in general industries.
Cures tack-free with up to 5,400 PSI on many different metals / glass / ceramics. Very low linear shrinkage with enhanced excellent moisture and temperature resistance. Good passive vibration isolation capability.
Metal / Glass / Ceramics
Clear
300 cP
4,400 to 5,400
D59 – D69
400%