880-5GALLON
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Chemical Type : Oxime
Color : Translucent
Viscosity : 800 – 1,200
Density (g/ml) : 1.02
Peel Strength (psi) : N.A.
Tensile Shear (psi) : 220
Elongation (%) : 315