Product Highlights         : One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured
                                            adhesive in shadowed areas. Used as conformal coating and sealant for PCBA and electronic components.

Cure Time                       : 24 hr, RT

Viscosity                         : 600

Temp. Resistance  (°C)  : -45 to 260

 Color                              : Clear

Tensile ( psi)                   : 100

 