109-500GM

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights            : Low odor / Low bloom, Medium-low viscosity, High humidity,Solvent-resistant and Bonds P,M

Substrates                          : Ultra-low Odor, Low-Bloom, High Strength Medical CA Bonder

Viscosity                             : 900 cps

Shear Strength                  : 2,920 psi

Bonding Strength (psi)

ABS                                    : 800

Aluminum                          : 2,300

PC                                      : 1,300

PVC                                    : 1,100

Rubber                              : -

Steel                                  : 3,000

 