CM-4-50GM
Product Availability: In stock
Product Highlights : Low odor / Low bloom, Ultra-low viscosity, Solvent-resistant, Bonding P,R,M and Medical grade
Substrates : Ultra-low Odor,Non-Bloom, High Strength Medical CA Bonder
Viscosity : 4 cps
Color : Clear
Bonding Strength (psi)
ABS : 800
Aluminum : 2,300
PC : 1,300
PVC : 1,100
Rubber : -
Steel : 3,000