CM-315B-500GM
Product Availability: 2 To 4 Weeks
Product Highlights : High Temp., Med. viscosity,Black, Rubber toughened, Bonds P,M, Medical grade and Thermal shock
Substrates : Ultra-High Temp, Superior Strength Medical CA Bonder
Viscosity : 315 cps
Color : Black
Bonding Strength (psi)
ABS : 2,500
Aluminum : 3,200
PC : 3,800
PVC : 3,200
Rubber : 2,200
Steel : 5,200