1049
Product Availability: 2 To 4 Weeks
Product Highlights :
Medium-high viscosity active alignment optical bonder. Used in optical/medical devices for bonding of metals, glass and ceramics. Very low shrinkage and water absorption. Ability to withstand stringent thermal cycling.
Substrates : High Performance Metal/Glass/Ceramics
Color : Clear Transparent
Viscosity : 4,500 - 7,500cps
Tensile (psi) : 10,100-10,800
Hardness : D80 - D90
Elongation : 44%