Product Highlights              : Two Part Epoxy, 100:12 Ratio. Aluminum-Filled, Ultra High-Temp, Low Shrinkage and High Thermal Conductivity.

Color                                     : Grey

Dielectric Strength              : 50 volts/mil

Viscosity (cPs)                     : 8,000 - 14,000

Hardness Shore                   : D87

Vol. Resistivity (ohms-cm) : 1.0 x 105

Chemical Resistance           : Good

 