UHTE-5321-5GALLON
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Single-Part Contact Adhesive, Excellent Flexibility.
Color : Black
Dielectric Strength : 300 volts/mil
Viscosity (cPs) : 25,000 - 45,000
Hardness Shore : N.D.
Vol. Resistivity (ohms-cm) : 1.0 x 1013
Chemical Resistance : Excellent