HTE-6498-1KG

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights                  : Two-component epoxy (sealant and encapsulant) bonding material. 3 mins fast-setting, strength starts increasing after 15 mins, full cure in 72hrs. High gloss black                                                         encapsulant, high temperature and chemical resistance.

Substrates                               : Multi-Substrates (High Strength) 

Color                                        : Clear

Tensile (psi)                            : 9,400

Flexural (psi)                          : 145,500 

Viscosity  (Mixed)                  : 14,500 cps

Cure (Shrinkage)                   : 0.0005 in/in 

Temperature  (Resistance)   : -55 to 155°C 

 