Product Highlights : Industrial grade, very low viscosity high strengthmulti-substrate bonder. Very useful for bonding of substrates with
                                    different hardness.

Substrates              : Multi-Substrates (High Strength Plastics)

Color                       : ClearTranslucent

Viscosity                : 250 cps

Tensile (psi)           : 2,400 - 6,800

Hardness               : D68 – D78

Elongation             :  310%

 