uvincure284

1404-5GALLON

Product Availability: 2 To 4 Weeks

Product Highlights : Medium viscosity, acid-free form-in-place gasket and sealant. Very low linear shrinkage. Ideal for medical optics
                                     positioning / alignment application. Adhere well to glass / metals / ceramics / plastics.

Substrates              : Multi-Substrates (High Strength Plastics)

Color                       : Slight Yellow Tint

Viscosity                 : 2,900 cps

Tensile (psi)            : 7,100

Hardness                : D67 - D77

Elongation              :  73%

 