Product Highlights : For porous materials, Gel viscosity, Ease of control and Solvent-resistant
Substrates : Bonds P,R,M High Strength, Multi-Substrates Structural CA Bonder
Viscosity : 11,500 cps
Shear Strength : 3,875 psi
Bonding Strength (psi)
ABS : 2,700
Aluminum : 2,000
PC : 3,700
PVC : 3,900
Rubber : 2,200
Steel : 2,800