328-500GM

Product Availability: In stock
CMB_04
$152.38

Product Highlights            : High Temp., Medium viscosity , Rubber Toughened, High strength on P,M and Thermal shock

Substrates                          : Ultra-High Temp, Superior Strength Medical CA Bonder

Viscosity                             : 500 cps

Color                                   : Clear

Bonding Strength (psi)

ABS                                    : 2,500

Aluminum                          : 3,200

PC                                      : 3,800

PVC                                    : 3,200

Rubber                              : 2,200

Steel                                  : 5,200

 

There are yet no reviews for this product.