TC-9033

Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)

Product Highlights                                     : Thermally Conductive, Aluminum-Filled, and 1:1 Epoxy Paste

Ratio                                                             : 1:1

Color                                                            : Grey

Viscosity Mixed  (cP)                                  : Paste

Volume Resistivity (ohms-cm)                  : 1.0 x 105

Dielectric Strength (volts/mil)                   : 80

Thermal Conductivity (Btu-in/hr-ft2-°F)   : 9.0

Temp. Resistance (°C)                                : 204

 