899-3OZ
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : A straw color gel silicone that is removable after cure. Clean release from plastics, metals and painted wood. Non-corrosive.
Color : Translucent
Appearance : Gel
Viscosity : 80,000
Tensile (psi) :100
Hardness : A30