uvincure44

3561-1KG

Product Availability: 2 To 4 Weeks

Product Highlights : conformal coating (30-150 microns) for PCBA. Use with high volume spray valve system, does not clog valves.
                                 Fluorescing feature for in-line inspection.

Substrates              : Multi-Substrates

Color                       : Yellow Tint, Fluorescing

Viscosity                : 225 cps

Tensile (psi)           : Good

Hardness               : D35 – D45

Elongation             :  74%

 