1283-5GALLON
Product Availability: 2 To 4 Weeks
Product Highlights : Cures with UV / Visible / Heat or Actif 398. Good clarity, heat and moisture resistance. Good passive vibration
isolation capability. Ideal for relays for circuit breakers in the electronics industry for outdoor use.
Substrates : High Performance Metal/Glass/Ceramics
Color : Clear
Viscosity : 600 cps/p>
Tensile (psi) : 5,700 - 9,800
Hardness : D68 – D78
Elongation : 55%