Product Highlights : Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal / glass / ceramics
                                    bonder. Low linear shrinkage, good weather-ability, temperature and moisture resistance.

Substrates              : High Performance Metal/Glass/Ceramics

Color                       : Slight Tint

Viscosity                : 130 cps

Tensile (psi)           : 7,400 – 10,000

Hardness               : D75– D85

Elongation             :  4%

 