4272-30GM

Product Availability: 2 To 4 Weeks
123412

Product Highlights : Aerospace Grade. Cures with UV / Visible / Heat or activator (Actif 398). Very low viscosity, high strength metal /
                                    glass / ceramics masking material. Low linear shrinkage, good temperature and moisture resistance.

Substrates              : High Performance Metal/Glass/Ceramics

Color                       : Slight Tint

Viscosity                 : 400 cps

Tensile (psi)            : 9,700 – 10,900

Hardness                : D77 – D87

Elongation              :  4%

 