6322-300GM
Product Availability: 2 To 4 Weeks
Product Highlights : Low viscosity, highly resilient (memory retention) and high flexibility out-perform many gaskets provides air-tight
sealing. Available in different colors.
Substrates : MultiSubstrates(Plastics)
Color : Transparent
Viscosity : 400 cps
Tensile (psi) : 2,400 - 4,000
Hardness : D17 – D27