uvincure395

6213-1GALLON

Product Availability: 2 To 4 Weeks

Product Highlights : Cost efficient epoxy-acrylate low viscosity, ultra-low shrinkage and water absorption potting compound for use in
                                    sensitive electronic devices. Chemical and vapour resistance.

Substrates              : Multi-Substrates (Low Adhesion)

Color                       : Transparent

Viscosity                 : 800 cps

Tensile (psi)            : 2,200 - 2,700

Hardness                : D55 – D65

Elongation              : 430%

 