3393VT-10GM
Product Availability: 2 To 4 Weeks
Product Highlights : Very thick, low water absorption electronics sealant. Provides air-tight seal with ease of peel for rework. Tough
yet elongating. Widely use for automotive and electronics industries for its low CTE properties.
Substrates : Very Low Strength Multi-Substrates
Color : Slightly Translucent
Viscosity : 20,000 cps
Tensile (psi) : 1,200 - 3,000
Hardness : A5 – A15
Elongation : 374%