Product Highlights :Cures with UV / Visible / Heat or Actif 398. Very high strength, medium viscosity metal / glass bonder. Low
shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption.
Color : Slight Tint
Viscosity : 1,850 cps
Tensile (psi) :9,500 – 16,000 psi
Hardness : D66 - D76
Elongation : 600%