5422T-5GALLON

Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work Singapore)

Product Highlights   : Medium viscosity, multi-substrate bonder for most plastics, metal and glass. Ideal for needle / reservoir /
                                     catheter / transducer assemblies in the medical industry. Formulated to meet ISO 10993-5. Passes EtO
                                      & gamma sterilization. 

Color                          : Clear

Viscosity                   : 5,000 cps

Tensile                      : 4,000 - 7,000 psi

Hardness                  : D60 - D70

Elongation                : 350% 

 