5005-1KG

Product Availability: 2 To 4 Weeks

Product Highlights : High-strength multi-substrate bonder. For medical devices with demanding applications. Offers adaptability,
                                    strength and rapid cure. Tough-yet-flexible material with high reliability. Passes EtO and gamma sterilisation.

Substrates              : High Strength Plastics

Color                       : Clear

Viscosity                : 3,500 – 5,500 cps

Tensile (psi)           : 3,200 – 6,900 psi

Hardness               : D51 – D61

Elongation             :  812%

 