7795-1KG
Product Availability: 2 To 4 Weeks
Product Highlights : Medium high viscosity, superior high strength bonder. Used for bonding of metals, glass and ceramics in
electronics / optical / medical devices. Very low shrinkage and water absorption. Ability to withstand stringent
thermal cycling
Substrates : High Performance Metal/Glass/Ceramics
Color : Slight Tint
Viscosity : 6,500cps
Tensile (psi) : 10,100 – 12,600
Hardness : D82 - D92
Elongation : 24%