5422F-2GALLON

Product Availability: 2 To 4 Weeks
Price Shown Is Per Each (Ex-Work Singapore)

Product Highlights : Low viscosity, multi-substrate bonder for most plastics, metal and glass. Ideal for needle / reservoir / catheter /
                                   transducer assemblies in the medical industry. Meet ISO 10993-5. Passes EtO & gamma
                                   sterilization.

Substrates              : Multi-Substrates

Color                       : Clear, Fluorescing

Viscosity                 : 200 – 400 cps

Tensile (psi)            :3,700 – 6,900

Hardness                : D57 to D67

Elongation              : 350%

 