1859-2GALLON
Product Availability: 2 To 4 Weeks
Product Highlights : Multi-substrate bonding gel for most plastics, metal and glass. Ideal for out-door bonding in general and
construction industries. Good passive vibration resistance. Enhanced thermal and water resistance
Substrates : Multi-Substrates (High Strength Plastics)
Color : Clear
Viscosity : 53,000 cps
Tensile (psi) : 6,900
Hardness : D63 - D73
Elongation : 110%