1404-10GM
Product Availability: 2 To 4 Weeks
Product Highlights : Medium viscosity, acid-free form-in-place gasket and sealant. Very low linear shrinkage. Ideal for medical optics
positioning / alignment application. Adhere well to glass / metals / ceramics / plastics.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Slight Yellow Tint
Viscosity : 2,900 cps
Tensile (psi) : 7,100
Hardness : D67 - D77
Elongation : 73%