Incure offers UV/LED light curable dome and decorative material coating material. Manufactured with various hardness, flexibility, dome profie and adhesion for different substrates, they exhibit good wetting capability for ease of application. Cures to a sleek and crystal clear surface, they have superior and long-lasting adhesion to metals, glass, wood, paper and plastics.

Dome coating materials are commonly used in decorative and novelty products such as name-plates, pens, decals, badges and logo stickers etc.

Designed with very low shrinkage and water absorption, they are good for stringent thermal cycling for long-lasting and durable performance.

Advantages of Cast-MaxTM - UV Dome Coatings

 Solvent Free
 Superior Environmental Resistance
 Tack-Free UV Cure In Seconds
 Wide Range of Viscosities

Learn about our Light Curing Systems

C9000 / U8000 UV Light Curing Conveyor Systems
F100P / F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED Flood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps
UV Casting
Cast-MaxTM Series Core Products
Product Product Highlights Substrates Color Viscosity Tensile Hardness Elongation  
2613 Low viscosity bonder. Used in gems and metal bonding for bracelets, necklaces, rings, penchants, hair clips, hair bands, earrings, crowns etc. Also used as dome coating of nameplates and logos.   - Water-White Clear 700 - 1,400 cP 4,700 - 5,200 psi  D83 to D93  30%
2664 Medium viscosity bonder. Used in gems and metal bonding for bracelets, necklaces, rings, penchants, hair clips, hair bands, earrings, crowns etc. Also used as dome coating of nameplates and logos.  - Water-White Clear 2,000 - 4,000 cP 4,700 - 5,200 psi  D79 to D89   30%
Package Size: 10 ml syringe / 30 ml syringe / 1 kg Bottle / 1 Gallon Pail / 2 Gallon Pail / 18 kg Pail
APPLICATION
dome coating
1. Dispense adhesive on labels/stickers.
UV Dome Coating
Sticker coated with Cast-MaxTM 2664.
UV Curing
2. Cure in F200P UV Flood Lamp for 10 seconds.
Casting Adhesives
Coated label.
UV Dome Coating
3. Completed.
UV Adhesive Casting