HIGH PERFORMANCE METAL ADHESIVES FOR METAL BONDING

Incure Quad-CureTM Metal Bonder offers a unique range of high performance metal adhesives for the ferrite, metals, motors and speakers industry. These adhesives cure completely between surfaces with activator or heat. Extremely versatile especially in areas where light cannot reach.

Advantages of Quad-CureTM - Metal Bonder

  Fixtures in Seconds!
  Room Temperature Cure
  Environmetally Resistant

Learn about our Light Curing Systems

C9000/ U8000 UV Light Curing Conveyor Systems
F100P/F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED lood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10/S20 Ultra High Intensity Light-Curing Spot Lamps
Ultra High Temp
Quad-CureTM Series Core Products
Product Product Highlights Color Viscosity Tensile Hardness Elongation  
9218
Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption. 
Slight Tint 
 
20,500 cP 8,000 – 8,200 psi D43 - D53 444
9245 Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption. 
Slight Tint  3,650 cP 6,800 – 10,000 psi D65 - D75 820
9254 Cures with UV / Visible / Heat or Actif 398. Very high strength, medium viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption. 
Slight Tint 1,850 cP 9,500 – 16,000 psi D66 - D76 600
9273 Cures with UV / Visible / Heat or Actif 398. Very high strength, high viscosity metal / glass bonder. Low shrinkage and good passive vibration isolation capability. Resistant to moisture and low water absorption. 
Slight Tint 950 cP 7,900 – 8,200 psi D40 - D50 544
398 Activator used in the absence of UV / Visible light source or between opaque substrates. Up to 70% bonding strength achievable within 5 mins. Maximum bonding strength at 72hours for use with quad-cureTM series only.  Slightly Yellow 6 cP - - -
Package Size: 10 ml syringe / 30 ml syringe / 1 kg Bottle / 1 Gallon Pail / 2 Gallon Pail / 18 kg Pail