LOW ODOR, LOW BLOOM CYANOACRYLATE ADHESIVES

Incure Quik-FixTM Low Bloom, Low Odor Cyanoacrylate Instant Adhesives offer the most diverse line of cyanoacrylate glue/instant adhesives available, providing you with fast assembly solutions for a variety of materials, including plastics, rubbers and metals. Cyanoacrylate is no mix product that cure rapidly at room temperature without light or heat, making it exceptionally easy to use.

Advantages of Quik-FixTM - Cyanoacrylate


  Single Component - Easy To Use
  Ultra Low Odor
  Reduce Inventory Costs - Used On Various Sizes
  Available in a Variety of Viscosities

Learn about our Light Curing Systems

C9000 / U8000 UV Light Curing Conveyor Systems
F100P / F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED Flood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps
Plastic Adhesives
Quik-FixTM Series Core Products
Product Product Highlights Substrates Viscosity Shear Strength Bonding Strength (psi)
ABS Aluminum PC PVC Rubber Steel  
 
109
 
• Low odor / Low bloom
• Medium-low viscosity
• High humidity
• Solvent-resistant
• Bonds P,M
Ultra-low Odor, Low-Bloom,
High Strength Medical
CA Bonder
900 cP 2,920 psi 800 2,300 1,300 1,100 -  3,000
520 • Low odor / Low bloom
• Ultra-low viscosity
• High humidity
• Solvent-resistant
• Bonds P,M
Ultra-low Odor, Low-Bloom,
High Strength Medical
CA Bonder
4 cP 2,920 psi 800 2,300 1,300 1,100 -  3,000
524 • Low odor / Low bloom
• Very low viscosity
• High humidity
• Solvent-resistant
• Bonds P,M
Ultra-low Odor, Low-Bloom,
High Strength Medical
CA Bonder
50 cP 2,920 psi 800 2,300 1,300 1,100 -  3,000
Package Size: 20g bottle / 500g bottle
Abbrv: P - Plastics, R - Rubber, M - Metals, F - Foam, C - Cloth, W - Wood