CONFORMAL COATING

UV LIGHT CURING CONFORMAL COATINGS FOR ELECTRONIC COMPONENT AND ASSEMBLY

Incure Ultra-IlluminaTM offers a range of conformal coatings for printed circuit boards protection. These UV conformal coatings cure tack free in seconds upon exposure to UV/Visible light to help streamline manufacturing assembly processes.

Fill in your Electronics Application Profile Here


Advantages of Ultra-IlluminaTM - Conformal Coatings

  Black Grades Available
  Low Stress Under Thermal Cycling
  Solvent Free
  Superior Environmental Resistance
  Tack-Free UV Cure In Seconds
  Wide Range of Viscosities

Learn about our Light Curing Systems

C9000 / U8000 UV Light Curing Conveyor Systems
F100P / F200P Programmable UV Flood Curing Lamps
L1000 High Intensity UV LED Flood Lamps
L9000 Compact UV LED Spot Curing Lamps
S10 / S20 Ultra High Intensity Light-Curing Spot Lamps

Ultra-IlluminaTM Series Core Products
Product Product Highlights Substrates Color Viscosity Tensile (psi) Hardness Elongation  
3502 Low viscosity, hard and resilient UV curable conformal coating (30-150 microns) for PCBA. Use with high volume spray valve system, does not clog valves. Fluorescing feature for in-line inspection. Multi-Substrates Clear
Fluorescing
350 cP Good D68 – D78 55%
3511 Low viscosity, clear, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA. Shadowed areas under components are cured with the secondary heat-cure process. Multi-Substrates Clear
Fluorescing
150 cP 4,400 
to
5,700
D59 – D69 400%
3511B Low viscosity, black opaque, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA. Shadowed areas under components are cured with the secondary heat-cure process. Multi-Substrates Opaque Black 160 cP 4,400 
to
5,700
D75 – D85 15%
3552 Low viscosity, clear, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA. Shadowed areas under components are cured with the secondary heat-cure process. Multi-Substrates Clear Fluorescing 400 cP 4,400 
to
5,700
D75 – D85 15%
5511 Low viscosity, clear, hard and glossy resilient medical grade UV curable conformal coating (30-500 microns) for PCBA.  Shadowed areas under components are cured with secondary heat-cure process. Multi-Substrates Clear Transparent,
Fluorescing
150 cP Good D75 – D85 15%
3561 Very low viscosity, hard and resilient UV curable conformal coating (30-150 microns) for PCBA. Use with high volume spray valve system, does not clog valves. Fluorescing feature for in-line inspection. Multi-Substrates Yellow Tint,
Fluorescing
225 cP Good D35 – D45 74%
Package Size: 10 ml syringe / 30 ml syringe / 30 ml squeeze bottle / 100 ml squeeze bottle / 250 ml squeeze bottle / 1 kg Bottle / 1 Gallon Pail / 2 Gallon Pail / 5 Gallon Pail

 

 

Results 31 - 36 of 36