F100 / F200

F100/F200 Compact UV Flood Curing Lamp

• Auto-Range AC Line Input • Standby Mode • Elapsed Hour Meter • Forced Air Cooling

The INCURE F100/200 is a compact UV flood curing lamp. F100/F200 integrates all system components into a small lamp head which can be easily mounted anywhere on a factory floor, with virtually no cabling or remote control boxes required. Just mount the head, connect the AC line cord, and start curing! The long life 400/600-Watt metal halide type lamp and parabolic reflector illuminate an 8 x 6 inch curing area with evenly distributed 100mW/cm2 UVA light (320–390nm). The arc lamp is powered by the state of the art UV Power-Plus Lamp Driver. The head features a convenient carrying handle and sliding height adjustment bracket.

uv_flood_curing_lamp
  F100/F200TM Series Core Products  
  Product Product Highlights Lamp Type Weight (lbs.)    
  F100

F100 integrates all system components into a small lamp head which can be easily mounted anywhere on a factory floor, with virtually no cabling or remote control boxes required

400 Watt Metal Halide 13 Pounds
  F200

F200 integrates all system components into a small lamp head which can be easily mounted anywhere on a factory floor, with virtually no cabling or remote control boxes required

600 Watt Metal Halide 13 Pounds
  Package Size: 10 ml syringe / 30 ml syringe / 30 ml squeeze bottle / 100 ml squeeze bottle / 250 ml squeeze bottle / 1 kg Bottle / 1 Gallon Pail / 2 Gallon Pail / 5 Gallon Pail  
Configuration F100 F200
Order Number 290005 290033
Input Voltage 90-132/180-265VAC 90-132/180-265VAC
Input Current, 120/240V 7A/3.5A maximum 10A/5.0A maximum
Source Input Frequency 47 Hz to 63 Hz   47 Hz to 63 Hz  
Lamp Power Regulation ± 1%   ± 1%  
Fan / Auxiliary Voltage 24V 24V
Lamp Type 400 Watt Metal Halide 600 Watt Metal Halide
Burning Position Horizontal Horizontal
Radiation Flux 110 Watts 110 Watts
Warm-up Time 2 minutes 2 minutes
Cooling time before Restart  5 minutes typical 5 minutes typical
Curing Area  8 x 6’’ minimum 8 x 6’’ minimum
Lamp Life 1000 hours typical  1000 hours typical 
Operating Temperature +10°C to +40°C
+50°F to +104°F
+10°C to +40°C
 +50°F to +104°F
Relative Humidity 30 to 75% operating, 10 to 100% storage 30 to 75% operating, 10 to 100% storage 
Cooling Forced air Forced air 
L x W x H (inches) 11” x 10” x 9” 11” x 10” x 9” 
Weight (lbs.) 13 Pounds 13 Pounds
 Download: Bulletin for F100/200 UV Flood Curing Systems (119 KB)